Packaging is a high-volume industry, and masterbatch selection weighs cost, line speed and shelf appearance together. Erk-Han produces filler, white and color masterbatches and process additives for flexible and rigid packaging makers, suitable for film extrusion, blow molding and injection molding.
You can explore all our product groups on the Erk-Han Masterbatch home page.
Recommended Dosage Rates and Technical Summary
Recommended Dosage
Flexible packaging and thin film: 1.0% – 2.5%
Rigid packaging, bottles and injection molding: 1.5% – 3.0%
High-opacity and food/barrier applications: 2.0% – 4.0%
Polymers
LDPE, LLDPE, HDPE, PP homopolymer and copolymer, clear PP, PET, PS and recycled (rPCR) polyolefins
Processes
Blown and cast film extrusion, multilayer film, film for vertical form-fill-seal (FFS) lines, blow molding, injection molding, thermoforming
Polymer Science, Working Mechanism and Field Examples for the Sector
Scientific Mechanism
The basic physical requirements of flexible and rigid food packaging are opacity that protects food from photo-oxidation through Mie light scattering (rutile TiO₂ refractive index n ≈ 2.73), low migration governed by Fick's laws of diffusion (EU 10/2011 overall migration limit <10 mg/dm²), and low-FPV (<1.5 bar/g) dispersion quality that prevents pinholes in thin films.
On high-speed vertical form-fill-seal (FFS) lines, the surface coefficient of friction (COF, ASTM D1894) and blocking force (ASTM D3354) are precisely balanced through erucamide/silica synergy.
Field Example
In thin packaging films for dairy, oil and dry food, combining high-rutile white with antiblock/slip provides a light barrier without screen clogging or pinholes; in clear PP food containers, haze is minimized with nucleator-compatible transparent series.
Products and what they do
Filler masterbatch: Reduces polymer use in bags and film and improves the print surface.
Slip and antiblock: Make film easier to open and help it run on packaging lines.
Antistatic: Reduces dust pick-up and static charge during packing.
Food contact packaging
For packaging that will touch food, product selection follows the regulations of the target market (for example the EU 10/2011 migration limits in the EU). State this use in your quotation request; the right series and the documents that ship with it are chosen accordingly. On request, we provide our raw material suppliers' FDA 21 CFR compliance declarations together with an Erk-Han declaration of compliance.
Recommended Dosage
In flexible packaging and thin film applications: 1.0% - 2.5%
In rigid packaging, bottle, and injection molding processes: 1.5% - 3.0%
In special packaging requiring food contact compliance and barrier properties: 2.0% - 4.0%
Shipping
Orders are loaded in Bursa OSB, 30 minutes from Gemlik Port. We work under EXW, FCA, FOB, CFR, CIF and DAP and prepare the CoA, MSDS and TDS as well as the ATR, EUR.1 and certificate of origin each shipment requires.
Erk-Han Solutions by Packaging Category
In packaging, the right masterbatch is selected according to the packaging category, polymer and production process. The leading Erk-Han solutions in the main categories are:
Flexible Food Packaging and Thin FilmsWhite masterbatch with high rutile TiO₂ content for a light barrier in dairy, oil and dry food films; slip and antiblock masterbatches that balance film opening and surface friction on high-speed packaging lines.
Clear PP Food Containers and TraysNucleator-compatible transparent masterbatch series to keep haze low, and low-dosage color recipes that do not spoil the crystal-clear appearance.
Fresh Produce and Cold Chain PackagingAnti-fog masterbatch that reduces droplet formation on the inner surface of the package and helps keep the contents visible.
Bottles, Caps and Rigid PackagingColor masterbatch recipes that ensure shade consistency between cap and body in blow molding and injection processes, and spectrophotometric color matching to your brand color.
Packaging with Recycled (rPCR) ContentHigh-opacity recipes that cover the gray tone of recycled raw material, and odor-eliminating masterbatch that reduces plastic odor.
Packaging Requiring HygieneAntimicrobial masterbatch that helps limit microbial growth on the packaging surface; suitability is verified by project-specific laboratory testing.
Common Field Problems in Packaging Production and Erk-Han Solutions
Pinholes and Screen Clogging in Thin FilmCause: undispersed pigment agglomerates and a high filter pressure value. Erk-Han solution: high-dispersion color and white masterbatches produced to an FPV < 1.5 bar/g target.
Film Not Opening and Blocking on the Packaging LineCause: an unbalanced surface coefficient of friction (COF) and blocking force. Erk-Han solution: slip and antiblock masterbatches tuned through erucamide and silica synergy.
Light-Induced Spoilage in Dairy and Oil ProductsCause: light passing through the package due to insufficient opacity. Erk-Han solution: a light barrier with high-rutile TiO₂ white masterbatch that makes Mie scattering efficient.
Migration Risk in Food PackagingCause: low-molecular-weight components prone to migrating into food. Erk-Han solution: pigment and carrier systems selected with the EU 10/2011 overall migration limit (10 mg/dm²) in mind, together with a food contact declaration.
Haze in Clear ContainersCause: incompatible pigment or carrier selection that impairs transparency. Erk-Han solution: minimizing haze with nucleator-compatible transparent series.
Shade Differences in the Brand Color Between BatchesCause: color approval based on visual checks and variable dosing. Erk-Han solution: spectrophotometric ΔE measurement in every lot and metamerism control under different light sources.
Supported Polymers and Production Processes
PolymersLDPE, LLDPE, HDPE, PP homopolymer and copolymer, clear PP, PET, PS and recycled (rPCR) polyolefins.
ProcessesBlown and cast film extrusion, multilayer film, blow molding, injection molding and thermoforming.
Combined (Combi-Batch) SolutionsColor can be combined in a single granule with additives such as slip, antiblock and antistatic as required; compatibility and dosage are verified by project-specific laboratory testing.
Erk-Han Laboratory Tests Specific to the Packaging Industry
The main checks carried out in the Erk-Han laboratory for packaging projects are:
FPV (Filter Pressure Value) TestNumerical measurement of the risk of pinholes and screen clogging in thin films; target value < 1.5 bar/g.
Spectrophotometric ΔE MeasurementColor difference control with a Konica Minolta spectrophotometer so that the brand color stays the same in every lot.
Opacity and Hiding Power CheckNumerical verification of the light barrier in white and colored films and containers.
MFI / MVR MeasurementVerification of the flow compatibility of the carrier resin with the base packaging polymer.
Ash Furnace AnalysisCheck in every batch that the pigment and TiO₂ content matches the recipe value.
Regulatory DocumentationEU 10/2011 / FDA food contact declaration of compliance together with REACH, RoHS and SVHC declarations.
A 54-question technical guide compiled from the field experience of the Erk-Han engineering team.
Which masterbatch is safe for food packaging?
Low-migration, heavy-metal-free Erk-Han food-grade series compliant with EU 10/2011, FDA and REACH; formulations that do not alter the taste, odor or composition of the food should be used.
How is light protection provided in milk and oil packaging?
With high-TiO2-content opacifying masterbatch; UV and visible light transmission is reduced to zero, extending the shelf life of the contents.
Why do micro-holes (pinholes) form in thin films (BOPP/CPP)?
This is caused by TiO2 agglomeration; a high-dispersion, fine-particle-size titanium masterbatch provides agglomerate-free distribution and a smooth surface.
How is blocking (sticking) prevented in packaging film?
With antiblock masterbatch; the silica-based additive creates micro-roughness on the film surface, preventing the layers from sticking to one another.
The films are not slipping/opening on the machine during bag production?
The coefficient of friction is high; adding slip masterbatch lowers the COF and increases the packaging line speed.
Based on what is the migration test performed in food packaging?
With the relevant food simulants within the framework of EU 10/2011; Erk-Han low-migration series meet these criteria.
What should the packaging masterbatch dosage generally be?
1-4% depending on the application; low for thin film, higher for opacifying/colored applications, adjusted according to the TDS.
How is glass-like clarity achieved in transparent packaging?
With transparent masterbatch containing a nucleating agent/clarifier; the haze value of PP/PE is minimized to provide glass-level transparency.
How is color matching (brand color) guaranteed in packaging?
With a spectrophotometer and tight ΔE tolerance; the brand color is produced consistently by measuring every lot.
How is the risk of color migration (bleeding) reduced in food film?
By using high-molecular-weight, low-migration pigments (e.g. PY151); color transfer to the food is prevented.
Does filler masterbatch affect film printing?
At the right ratio the effect is positive: calcite gives a matte surface and improves ink adhesion. In very thin films, puncture and tear resistance limit the ratio.
The layers stick when the film roll is opened. What should I use?
An antiblock additive creates micro-roughness on the film surface and stops the layers from sticking; a slip additive lowers surface friction. The two are often used together.
What information should I give for food packaging?
The target market, the type of food to be packed and the use temperature. The series is selected from this information; in the EU, the EU 10/2011 framework applies.
Which delivery terms do you work with?
EXW, FCA, FOB, CFR, CIF and DAP. Just state the delivery term and the port of destination in your quotation request.
How is odor (originating from rPCR) removed from packaging?
With odor-absorbing masterbatch; VOC and aldehyde/amine-based molecules are trapped through chemical neutralization to obtain an odorless product.
Why is the strength low in garbage bags/industrial bags?
The filler/pigment dispersion is poor; a masterbatch with homogeneous distribution that preserves tensile and puncture strength should be selected.
Why do streaks (die lines) occur in packaging film?
Die contamination or coarse particles; resolved with a clean die, a suitable filter and a high-purity masterbatch.
How is antistatic packaging (for electronics) produced?
With antistatic masterbatch; surface resistivity is lowered to prevent dust attraction and static discharge, protecting sensitive electronics.
How is whiteness and opacity increased in food containers?
With white masterbatch containing high TiO2 (50-80%); absolute opacity and bright whiteness are achieved at low dosage.
How is the UV resistance of packaging film increased?
With UV stabilizer (HALS) masterbatch; color fading and embrittlement are delayed in packaging stored outdoors.
How is color homogeneity ensured in bottle (blow molding) production?
With high-dispersion masterbatch and correct dosage; uniform color and a smooth surface are obtained throughout the bottle wall thickness.
Is coloring possible for biodegradable packaging?
With PLA/PBAT-compatible biopolymer masterbatch; environmentally friendly color solutions are offered while EN 13432 compostability is preserved.
Why is a gel (fish-eye) defect seen in packaging film?
Burnt polymer or coarse gel; prevented with a controlled process, a clean filter and a gel-free masterbatch.
How is a metallic/pearlescent packaging effect achieved?
With special effect masterbatch (pearlescent/metallic); an aesthetic shimmer is provided for luxury packaging and cosmetics.
How is layer compatibility ensured in multilayer film?
With masterbatch carried in a carrier suited to each layer's polymer; delamination and color shift are prevented.
What is the safety regulation for toy packaging?
Compliance with EU 10/2011, REACH and RoHS; heavy-metal-free, safe Erk-Han series should be used.
Is cling in stretch film affected by coloring?
The wrong additive impairs cling; a cling-compatible special masterbatch that does not alter surface energy should be selected.
How is the carbon footprint reduced in packaging?
With recycled (PCR) polymer-compatible masterbatch and biopolymer series; sustainable production is supported.
How is a gray/dirty tone corrected in rPCR packaging?
With toner and opacifying masterbatch; a neutral base is created so that the target color is achieved cleanly.
Which pigment is used in food-contact black packaging?
Food-compatible, low-PAH carbon black masterbatch; standard blacks may not be suitable for food contact.
How is optical brightness increased in packaging film?
With optical brightening agent (OBA) masterbatch; yellowing is masked to provide a brighter white perception (food compliance must be checked).
Why do flow marks occur in injection-molded container production?
This is a dispersion or mold temperature issue; resolved with a homogeneous masterbatch and optimized mold temperature.
Is antimicrobial protection necessary in packaging?
Yes for hygiene-critical food containers; a silver-ion-based, ISO 22196-compliant antimicrobial masterbatch can be used.
The color lightens as the film thickness decreases, what is the solution?
Color strength must be balanced with dosage; in thin film, the target color depth is maintained with a more concentrated masterbatch.
Why is the carrier polymer important in packaging masterbatch?
PE carrier for PE film, PP carrier for PP; incompatibility creates gels, haze and mechanical weakness.
Is the barrier property impaired by coloring in vacuum packaging?
Yes, if a suitable additive is not selected; oxygen/moisture permeability is preserved with a barrier-compatible masterbatch.
How is scrap reduced on a high-speed film line?
With low-FPV, clean masterbatch; filter clogging and downtime are reduced, lowering scrap.
Why does heat-related yellowing occur in packaging?
This is thermo-oxidative degradation; the melt is stabilized with an antioxidant-additive masterbatch to prevent yellowing.
Why do white specks appear in packaging film?
Contamination or poor distribution; resolved with a high-purity, well-dispersed masterbatch.
How is color consistency ensured in colored closures?
With injection-compatible, heat-stable masterbatch; the color difference from mold to mold is minimized.
Can fluorescent warning colors be used in packaging?
Yes, with fluorescent masterbatch; however, since light fastness is limited, they are suitable for short-shelf-life applications.
Does crystallization in a PET tray affect coloring?
If a suitable pigment is not selected, haze increases; a PET-compatible masterbatch that does not disrupt crystallization should be preferred.
How should packaging masterbatch be stored?
In a cool, dry environment, in its original packaging; moisture-absorbing carriers should be dried before production.
What happens when the TiO2 ratio is increased in thin packaging?
Opacity increases, but in excess a risk of embrittlement and pinholes arises; the optimum concentration is selected according to the TDS.
Why do layer thickness fluctuations occur in packaging film?
Feeding or melt inhomogeneity; stabilized with gravimetric dosing and low-FPV masterbatch.
How is a luxury appearance achieved in cosmetic packaging?
With metallic, pearlescent and high-gloss effect masterbatches; premium aesthetics and brand value are enhanced.
What is the single-polymer (mono-material) trend for recycling in packaging?
Masterbatch compatible with mono-PE or mono-PP structures; it increases recyclability while preserving color/barrier properties.
The packaging film is tearing during packaging?
The strength is low; a well-dispersed masterbatch that preserves tensile strength and the correct dosage should be used.
How is it guaranteed that additives do not migrate into the food in food film?
With low-migration, regulation-compliant formulations and migration tests; full traceability is ensured.
What if a natural appearance is desired instead of opaque white in packaging?
With low-TiO2 or transparent masterbatch; a natural/matte aesthetic and partial transparency are achieved.
How is color durability ensured in hot-fill packaging?
With heat-stable pigments; the TDS heat resistance is checked so that no color shift occurs at the filling temperature.
How can a sample and TDS be obtained for a packaging project?
You can request a sample and technical documentation by applying to the Erk-Han laboratory with information on the polymer type, film/mold process and target color.
Who determines the correct packaging masterbatch?
Erk-Han sales engineers; they recommend the optimum safe series according to food compliance, process and aesthetic requirements.
How are scratches and surface matting prevented in packaging?
With slip agent and correct dosage; surface friction is reduced to prevent scratching and matting during handling/packaging.
Let's find the right solution for your project
Contact our team for sample requests, color matching or technical consultancy.